Abstract
Surface analysis techniques have been used to investigate tin oxide-coated soda lime glass specimens prior and subsequent to their exposure to DC bias, heat, and humidity. All specimens reported here comprise the following layered structure: tin oxide/silicon oxycarbide/glass. Depth profiling using X-ray photoelectron spectroscopy (XPS) clearly shows the interfacial regions in both controlsamples and samples exposed to the above-mentioned conditions (stressed). Control samples show distinct and relatively compact interfacial regions as well as an intact silicon oxycarbide diffusion barrier. Stressed films, however, show more diffuse interfacial regions and a physically and chemically altered silicon oxycarbide diffusion barrier. This deterioration of the diffusion barrier isproposed to be a pre-requisite event to enable tin oxide delamination.
| Original language | American English |
|---|---|
| Number of pages | 7 |
| State | Published - 2003 |
| Event | National Center for Photovoltaics (NCPV) and Solar Program Review Meeting - Denver, Colorado Duration: 24 Mar 2003 → 26 Mar 2003 |
Conference
| Conference | National Center for Photovoltaics (NCPV) and Solar Program Review Meeting |
|---|---|
| City | Denver, Colorado |
| Period | 24/03/03 → 26/03/03 |
NLR Publication Number
- NREL/CP-520-33602
Keywords
- delamination
- thin films
- transparent conducting oxides (TCO)
- x-ray photoelectron spectroscopy (XPS)
Fingerprint
Dive into the research topics of 'Surface Analysis of Stressed and Control Tin Oxide Thin Films on Soda Lime Glass'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver