Surface Analysis: Measurements and Characterization (Brochure)

    Research output: NLRBrochure

    Abstract

    This brochure presents the capabilities that the Measurements and Characterization Division has in Surface Analysis, in which ia variety of spectrometry and spectroscopy techniques are used to determine the chemical, elemental, and molecular composition of material surfaces and interfaces.
    Original languageAmerican English
    PublisherNational Laboratory of the Rockies (NLR)
    Number of pages4
    StatePublished - 2000