In2S3 Atomic Layer Deposition and Its Application as a Sensitizer on TiO2 Nanotube Arrays for Solar Energy Conversion

  • Shaibal Sarkar
  • , Jin Young Kim
  • , David Goldstein
  • , Nathan Neale
  • , Kai Zhu
  • , C. Elliott
  • , Steven George
  • University of Colorado Boulder
  • National Renewable Energy Laboratory
  • Colorado State University

Research output: Contribution to journal › Article › peer-review

Original languageAmerican English
Pages (from-to)8032-8039
Number of pages8
JournalJournal of Physical Chemistry C
Volume114
Issue number17
DOIs
StatePublished - 2010

NLR Publication Number

  • NREL/JA-590-48501

Keywords

  • atomic layer deposition
  • quantum efficiencey
  • X-ray reflectivity
  • XRR

Fingerprint

Dive into the research topics of 'In2S3 Atomic Layer Deposition and Its Application as a Sensitizer on TiO2 Nanotube Arrays for Solar Energy Conversion'. Together they form a unique fingerprint.