Skip to main navigation Skip to search Skip to main content

Effects of Atomic Layer Deposition of Al2O3 on the Li[Li0.20Mn0.54Ni0.13Co0.13]O2 Cathode for Lithium-Ion Batteries

  • Yoon Seok Jung
  • , Andrew Cavanagh
  • , Yanfa Yan
  • , Steven George
  • , Arumugam Manthiram
  • University of Texas at Austin
  • University of Colorado Boulder
  • National Renewable Energy Laboratory

Research output: Contribution to journal › Article › peer-review

Original languageAmerican English
Pages (from-to)A1298-A1302
JournalJournal of the Electrochemical Society
Volume158
Issue number12
DOIs
StatePublished - 2011

NLR Publication Number

  • NREL/JA-5900-53725

Keywords

  • energy storage
  • hybrid electric vehicles
  • lithium-ion batteries