Differential Scanning Calorimetry Analysis of an Enhanced LiNi(0.8)Co(0.2)O(2) Cathode with Single Wall Carbon Nanotube Conductive Additives

  • Matthew Ganter
  • , Roberta DiLeo
  • , Christopher Schauerman
  • , Reginald Rogers
  • , Brian Landi
  • , Ryne Raffaelle
    • Rochester Institute of Technology
    • National Renewable Energy Laboratory

    Research output: Contribution to journal › Article › peer-review

    Original languageAmerican English
    Pages (from-to)7272-7277
    Number of pages6
    JournalElectrochimica Acta
    Volume56
    Issue number21
    DOIs
    StatePublished - 2011

    NLR Publication Number

    • NREL/JA-5200-52953

    Keywords

    • additive
    • battery
    • DSC
    • lithium
    • nanotube

    Cite this