Atomic Layer Deposition with TiO2 for Enhanced Reactivity and Stability of Aromatic Hydrogenation Catalysts

  • W. McNeary
  • , Sean Tacey
  • , Gabriella Lahti
  • , Davis Conklin
  • , Kinga Unocic
  • , Eric Tan
  • , Evan Wegener
  • , Tugce Erden
  • , Staci Moulton
  • , Chris Gump
  • , Jessica Burger
  • , Michael Griffin
  • , Carrie Farberow
  • , Michael Watson
  • , Luke Tuxworth
  • , Kurt Van Allsburg
  • , Arrelaine Dameron
  • , Karen Buechler
  • , Derek Vardon
  • National Renewable Energy Laboratory
  • Oak Ridge National Laboratory
  • Argonne National Laboratory
  • Johnson Matthey
  • Forge Nano

Research output: Contribution to journalArticlepeer-review

42 Scopus Citations

Abstract

Hydrogenation of aromatic molecules in fossil- and bio-derived fuels is essential for decreasing emissions of harmful combustion products and addressing growing concerns around urban air pollution. In this work, we used atomic layer deposition to significantly enhance the hydrogenation performance of a conventional supported Pd catalyst by applying an ultrathin coating of TiO2in a scalable powder coating process. The TiO2-coated catalyst showed substantial gains in the conversion of multiple aromatic molecules, including a 5-fold improvement in turnover frequency versus the uncoated catalyst in the hydrogenation of naphthalene. This activity enhancement was maintained upon scaling the coating synthesis process from 3 to 100 g. Based on the results from Xray photoelectron spectroscopy, X-ray absorption spectroscopy, and computational modeling, the activity enhancement was attributed to ensemble effects resulting from partial TiO2coverage of the Pd surface rather than fundamental changes to the Pd electronic structure. Additional durability testing confirmed that the TiO2coating improved the thermal and hydrothermal stability of the catalyst as well as tolerance toward sulfur impurities in the reactant stream. Using an economic model of an industrial deep hydrogenation process, we found that an increase in catalyst activity or lifetime of 2× would justify even a relatively high estimate for the cost of TiO2atomic layer deposition coatings at scale.

Original languageAmerican English
Pages (from-to)8538-8549
Number of pages12
JournalACS Catalysis
Volume11
Issue number14
DOIs
StatePublished - 2021

Bibliographical note

Publisher Copyright:
© 2021 American Chemical Society. All rights reserved.

NLR Publication Number

  • NREL/JA-5100-78670

Keywords

  • Aromatic hydrogenation
  • Atomic layer deposition
  • Catalysts
  • Coatings
  • Fuels