Skip to main navigation Skip to search Skip to main content

Atomic Layer Deposition for Aligned Growth of and Conformal Deposition onto Double and Triple Walled Carbon Nanotubes: Paper No. 776108

  • Colorado School of Mines
  • National Renewable Energy Laboratory
  • Rensselaer Polytechnic Institute

Research output: Contribution to conferencePaper

Original languageAmerican English
Number of pages7
DOIs
StatePublished - 2010
EventCarbon Nanotubes, Graphene, and Associated Devices III: SPIE Conference, 1-2 and 4 August 2010, San Diego, California, Graphene, and Associated Devices III: SPIE Conference - San Diego, California
Duration: 1 Aug 20104 Aug 2010

Conference

ConferenceCarbon Nanotubes, Graphene, and Associated Devices III: SPIE Conference, 1-2 and 4 August 2010, San Diego, California, Graphene, and Associated Devices III: SPIE Conference
CitySan Diego, California
Period1/08/104/08/10

NLR Publication Number

  • NREL/CP-520-49774

Keywords

  • aligned carbon nanotubes
  • atomic layer deposition
  • catalysts
  • fuel cells
  • iron
  • platinum

Fingerprint