Skip to main navigation Skip to search Skip to main content

Al2O3 Atomic Layer Deposition on Nanostructured ..gamma..-Mg(BH4)2 for H2 Storage

  • Noemie Marius
  • , Nicholas Strange
  • , Andreas Schneemann
  • , Vitalie Stavila
  • , Karl Gross
  • , Nancy Washton
  • , Madison Martinez
  • , Thomas Gennett
  • , Steven Christensen
  • Sandia National Laboratories
  • H2 Technology Consulting
  • Pacific Northwest National Laboratory
  • National Renewable Energy Laboratory

Research output: Contribution to journal › Article › peer-review

24 Scopus Citations

Abstract

In the context of the growing hydrogen (H2) economy, the demand for H2 storage materials is high, and metal borohydrides are of particular interest. Magnesium borohydride, Mg(BH4)2, has one of the highest hydrogen capacities of all known metal hydrides (14.9 wt % H) but suffers from high operating temperatures, slow kinetics for (de)hydrogenation, and the loss of capacity upon cycling. Strategies to address these challenges include nanoencapsulation and the use of chemical additives. This work is the first to utilize these two strategies simultaneously by using atomic layer deposition (ALD). For this new approach to modify borohydrides, we chose the well-studied Al2O3 ALD process using trimethylaluminum and water. Although there has been limited use of aluminum-based additives for Mg(BH4)2, we demonstrate that the low-temperature H2 capacity was doubled, desorption kinetics were increased by a factor of 3, and 100 cycles of Al2O3 suppressed the release of diborane compared to the uncoated Mg(BH4)2. We identified that the use of trimethylaluminum and water in the ALD process affected the decomposition pathway and that the Al2O3 film growth is dominated by infiltration due to the high porosity of the ..gamma..-phase Mg(BH4)2. From these results, the potential of ALD as a method to functionalize solid-state H2 storage materials is inferred, and recommendations for future ALD processes are presented.
Original languageAmerican English
Pages (from-to)1150-1162
Number of pages13
JournalACS Applied Energy Materials
Volume4
Issue number2
DOIs
StatePublished - 2021

NLR Publication Number

  • NREL/JA-5900-77649

Keywords

  • atomic layer deposition
  • hydrogen storage
  • magnesium borohydride

Fingerprint

Dive into the research topics of 'Al2O3 Atomic Layer Deposition on Nanostructured ..gamma..-Mg(BH4)2 for H2 Storage'. Together they form a unique fingerprint.

Cite this